Hommel Frit 482

Barium zinc frit

OxideAnalysisFormula
BaO4.13%0.072
CaO2.27%0.109
MgO3.41%0.227
K2O3.24%0.092
Na2O5.31%0.230
ZnO6.96%0.229
PbO3.36%0.040
TiO20.71%0.024
Al2O312.60%0.332
B2O33.19%0.123
SiO254.82%2.448
Oxide Weight268.37
Formula Weight268.37
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.0 x 10-6
GSPT - Frit Softening Point 1750F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 482" descrip="Barium zinc frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.130" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.270" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.410" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.240" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.310" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="6.960" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="3.360" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.710" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.190" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.820" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved