Hommel Frit 446

Leadless zinc high boron frit

OxideAnalysisFormula
CaO4.35%0.180
Na2O10.66%0.398
ZnO14.82%0.422
B2O328.73%0.957
SiO241.44%1.598
Oxide Weight231.73
Formula Weight231.73
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 446" descrip="Leadless zinc high boron frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.350" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.660" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="14.820" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="28.730" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="41.440" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved