Hommel Frit 441

Low lead calcium zinc borate frit

OxideAnalysisFormula
BaO1.50%0.032
CaO7.03%0.404
MgO0.38%0.030
K2O1.19%0.041
Na2O2.76%0.144
ZnO2.35%0.093
PbO17.71%0.256
Al2O39.04%0.286
B2O35.60%0.260
SiO252.44%2.816
Oxide Weight322.69
Formula Weight322.69
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.1 x 10-6
GSPT - Frit Softening Point 1640F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 441" descrip="Low lead calcium zinc borate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="1.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.030" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.380" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.190" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.760" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.350" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="17.710" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.040" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.440" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved