Hommel Frit 432

OxideAnalysisFormula
CaO6.14%0.279
MgO1.59%0.101
K2O6.63%0.180
Na2O3.07%0.126
ZnO10.00%0.314
Al2O313.27%0.332
B2O34.75%0.174
SiO251.58%2.191
ZrO22.97%0.062
Oxide Weight255.33
Formula Weight255.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.9 x 10-6
MLRG - Frit Melting Range (C) 1600F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 432" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.140" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.590" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.630" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.070" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.270" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.750" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.580" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="2.970" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved