Hommel Frit 419

OxideAnalysisFormula
CaO5.97%0.301
K2O2.36%0.071
Na2O4.03%0.184
ZnO8.60%0.299
PbO11.41%0.145
Al2O37.49%0.208
B2O36.58%0.268
SiO253.56%2.523
Oxide Weight283.09
Formula Weight283.09
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.9 x 10-6 (50-450C)
GSPT - Frit Softening Point 1700F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 419" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.970" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.360" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.030" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="8.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="11.410" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.490" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.580" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.560" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved