Hommel Frit 381

OxideAnalysisFormula
CaO10.95%0.496
PbO44.27%0.504
Al2O34.04%0.101
B2O35.45%0.199
SiO235.28%1.492
Oxide Weight254.09
Formula Weight254.09
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.6 x 10-6 (50-450C)
GSPT - Frit Softening Point 1305F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 381" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.950" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="44.270" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.040" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.450" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.280" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved