Hommel Frit 361

OxideAnalysisFormula
BaO2.46%0.052
CaO4.06%0.236
Li2O2.26%0.248
K2O1.96%0.068
Na2O6.47%0.341
ZnO1.37%0.055
Al2O33.81%0.122
B2O326.13%1.226
SiO251.49%2.798
Oxide Weight326.56
Formula Weight326.56
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.3 x 10-6
MLRG - Frit Melting Range (C) 1300F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 361" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.460" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.060" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.260" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.960" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.470" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.370" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.810" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.130" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.490" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved