Hommel Frit 2GF176D

LEADED

OxideAnalysisFormula
CaO5.25%0.338
K2O2.03%0.078
Na2O1.76%0.102
F3.53%0.670
PbO29.83%0.482
Al2O33.12%0.110
B2O311.93%0.618
SiO241.37%2.484
ZrO21.18%0.035
Oxide Weight360.79
Formula Weight360.79
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 2GF176D" descrip="LEADED" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.250" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.030" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.760" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="3.530" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="29.830" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.120" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.930" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="41.370" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="1.180" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved