Hommel Frit 285

Leadless Alkaline Frit

OxideAnalysisFormula
K2O2.99%0.100
Na2O17.68%0.900
Al2O36.79%0.210
B2O320.73%0.940
SiO251.81%2.720
Oxide Weight315.55
Formula Weight315.55
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 285" descrip="Leadless Alkaline Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.990" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="17.680" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.790" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.730" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.810" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved