Hommel Frit 27

OxideAnalysisFormula
CaO3.04%0.186
Na2O6.36%0.353
F1.24%0.224
PbO29.94%0.461
TiO28.86%0.381
B2O36.24%0.308
SiO244.32%2.535
Oxide Weight343.75
Formula Weight343.75
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.2 x 10-6 (50-450C)
GSPT - Frit Softening Point 1650F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 27" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.360" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="1.240" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="29.940" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="8.860" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.240" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.320" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved