Hommel Frit 259

Leadless, use for cone 06-02

OxideAnalysisFormula
CaO0.27%0.016
K2O6.04%0.208
Na2O14.14%0.739
ZnO0.94%0.037
F1.45%0.247
Al2O311.75%0.373
B2O316.50%0.768
SiO248.91%2.638
Oxide Weight324.10
Formula Weight324.10
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.30
GSPT - Frit Softening Point 1500F
MLRG - Frit Melting Range (C) 1500F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 259" descrip="Leadless, use for cone 06-02" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.270" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.140" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.940" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="1.450" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.750" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.910" tolerance=""/> </oxides> </material>