1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Hommel Frit 240

Oxide Analysis Formula
Na2O 6.40% 0.28
PbO 59.27% 0.72
B2O3 14.38% 0.56
SiO2 19.95% 0.90
Oxide Weight 271.17
Formula Weight 271.17