Hommel Frit 22

Low Lead Frit Boron Frit

OxideAnalysisFormula
CaO6.83%0.470
PbO30.65%0.530
B2O317.67%0.980
SiO244.85%2.881
Oxide Weight386.00
Formula Weight386.00
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 22" descrip="Low Lead Frit Boron Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.830" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.650" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.670" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.850" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved