Hommel Frit 13

High Lead Frit

OxideAnalysisFormula
Na2O8.21%0.300
PbO68.94%0.700
B2O311.98%0.390
SiO210.87%0.410
Oxide Weight226.61
Formula Weight226.61
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 13" descrip="High Lead Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.210" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="68.940" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.980" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="10.870" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved