Heraeus Schauer Frit K 1562

Lead sodium zero alumina frit

OxideAnalysisFormula
Na2O10.58%0.499
PbO38.24%0.501
Al2O30.10%0.003
SiO251.07%2.485
Oxide Weight292.42
Formula Weight292.42
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Heraeus Schauer Frit K 1562" descrip="Lead sodium zero alumina frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.580" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="38.241" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.105" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.074" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved