OxideAnalysisFormula
CaO0.42%0.073
MgO0.05%0.012
K2O3.34%0.344
Na2O3.56%0.557
P2O50.22%0.015
TiO20.05%0.006
Al2O314.06%1.336
SiO277.39%12.483
Fe2O30.20%0.012
Oxide Weight962.55
Formula Weight962.55
If this formula is not unified correctly please contact us.

Formulated as a substitute for UK Cornwall Stone for use in North America.

This was described in an article in Ceramics Technical Nov 2011. The chemistry has some significant differences to the standard UK Cornwall Stone (e.g. 5% more SiO2, 0.4% CaO vs. 1.8%, 6.9% KNaO vs. 7.6%). These suggest that it will not melt as quite as well, testing should be done.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="H&G Cornwall Stone" descrip="Synthetic version of UK Cornwall stone" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.340" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.560" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.220" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.050" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="14.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="77.390" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved