Glaze Spar #54

SODA FELDSPAR

OxideAnalysisFormula
CaO1.04%0.104
K2O1.51%0.090
Na2O8.92%0.805
Al2O322.48%1.234
SiO266.02%6.148
Oxide Weight559.63
Formula Weight559.63
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glaze Spar #54" descrip="SODA FELDSPAR" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.046" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.519" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.923" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.485" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.027" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved