•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Glaze A Ball Clay

Glasze suspender, hardener

A fine-grained engineered blend designed to provide excellent suspension, fired color, and film strength in a wide variety of ceramic glaze applications.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glaze A Ball Clay" descrip="Glasze suspender, hardener" searchkey="" loi="0.00" casnumber="70694-09-6"> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved