OxideAnalysisFormula
CaO7.80%0.302
K2O13.00%0.299
Na2O11.40%0.399
Al2O31.40%0.030
SiO266.40%2.397
Oxide Weight216.96
Formula Weight216.96
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 141 x 10-7
GSPT - Frit Softening Point 503C
MLRG - Frit Melting Range (C) 800-1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten M1233" descrip="Bleifreie Alkali-Fritte" searchkey="M 1233,M-1233" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved