Glasurfritten 37.06

Bleifreie Barium-Fritte

Alternate Names: 37 06,37-06

OxideAnalysisFormula
BaO47.00%1.000
Al2O317.00%0.544
SiO236.00%1.954
Oxide Weight326.17
Formula Weight326.17
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 70 x 10-7
MLRG - Frit Melting Range (C) 1180-1280C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 37.06" descrip="Bleifreie Barium-Fritte" searchkey="37 06,37-06" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="47.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved