Glasurfritten 37.031

Bleifreie Kalzium-Borat-Fritte

Alternate Names: 37 031,37-031

OxideAnalysisFormula
BaO55.40%0.313
CaO44.60%0.687
Oxide Weight86.48
Formula Weight86.48
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 85 x 10-7
GSPT - Frit Softening Point 610C
MLRG - Frit Melting Range (C) 700-1150C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 37.031" descrip="Bleifreie Kalzium-Borat-Fritte" searchkey="37 031,37-031" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="55.400" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="44.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved