Glasurfritten 37.025

Bleifreie Alkali-Bor-Fritte

Alternate Names: 37 025,37-025

OxideAnalysisFormula
Na2O15.00%1.000
B2O334.00%2.019
SiO251.00%3.507
Oxide Weight413.33
Formula Weight413.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 82 x 10-7
GSPT - Frit Softening Point 548C
MLRG - Frit Melting Range (C) 900-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 37.025" descrip="Bleifreie Alkali-Bor-Fritte" searchkey="37 025,37-025" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="34.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved