Glasurfritten 37.024

Bleifreie Alkali-Fritte

Alternate Names: 37 024,37-024

OxideAnalysisFormula
CaO3.00%0.112
K2O2.00%0.044
Na2O19.00%0.639
ZnO8.00%0.205
Al2O32.00%0.041
SiO266.00%2.291
Oxide Weight208.58
Formula Weight208.58
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 110x10-7
GSPT - Frit Softening Point 565C
MLRG - Frit Melting Range (C) 980-1060C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 37.024" descrip="Bleifreie Alkali-Fritte" searchkey="37 024,37-024" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="19.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="8.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved