Glasurfritten 35.32

Blei-Bor-Silikat-Fritte

Alternate Names: 35 32,35-32

OxideAnalysisFormula
PbO68.57%1.000
B2O319.80%0.926
SiO211.63%0.630
Oxide Weight325.51
Formula Weight325.51
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 75 x 10-7
GSPT - Frit Softening Point 473C
MLRG - Frit Melting Range (C) 800-1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 35.32" descrip="Blei-Bor-Silikat-Fritte" searchkey="35 32,35-32" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="68.570" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="11.630" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved