Glasurfritten 35.2

Bleihaltige Zinkmatt-Fritte

Alternate Names: 35 2,35-2

OxideAnalysisFormula
CaO5.00%0.160
Na2O2.00%0.058
ZnO27.00%0.596
PbO23.00%0.185
Al2O32.00%0.035
B2O34.00%0.103
SiO237.00%1.107
Oxide Weight179.82
Formula Weight179.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 61 x 10-7
GSPT - Frit Softening Point 600C
MLRG - Frit Melting Range (C) 970-1030C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 35.2" descrip="Bleihaltige Zinkmatt-Fritte" searchkey="35 2,35-2" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="27.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="23.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="37.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved