Glasurfritten 35.055

Bleimonosilikat-Fritte

Alternate Names: 35 055,35-055

OxideAnalysisFormula
PbO78.80%1.000
SiO221.20%0.999
Oxide Weight283.25
Formula Weight283.25
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 90 x 10-7
GSPT - Frit Softening Point 455C
MLRG - Frit Melting Range (C) 900-1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 35.055" descrip="Bleimonosilikat-Fritte" searchkey="35 055,35-055" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="78.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved