Glasurfritten 34.41

Blei-Aluminium-Silikat-Fritte

Alternate Names: 34 41,34-41

OxideAnalysisFormula
PbO74.56%1.000
Al2O34.78%0.140
SiO220.66%1.029
Oxide Weight299.36
Formula Weight299.36
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 77 x 10-7
GSPT - Frit Softening Point 500C
MLRG - Frit Melting Range (C) 900-1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 34.41" descrip="Blei-Aluminium-Silikat-Fritte" searchkey="34 41,34-41" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="74.560" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.780" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="20.660" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved