Glasurfritten 33.17

Bleifreie Zirkomfritte

Alternate Names: 33 17,33-17

OxideAnalysisFormula
BaO8.00%0.114
MgO1.00%0.054
K2O3.00%0.070
Na2O14.00%0.494
ZnO10.00%0.269
Al2O316.00%0.343
SiO248.00%1.746
Oxide Weight218.58
Formula Weight218.58
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 90x10-7 603C
GSPT - Frit Softening Point 603C
MLRG - Frit Melting Range (C) 1000-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glasurfritten 33.17" descrip="Bleifreie Zirkomfritte" searchkey="33 17,33-17" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="8.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved