Glassil A

OxideAnalysisFormula
Na2O27.00%1.000
SiO254.00%2.063
LOI19.00
Oxide Weight186.00
Formula Weight229.63
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Glassil A" descrip="" searchkey="" loi="19.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="27.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="19.000" tolerance=""/> </volatiles> </material>