Gerstley Bor (99)

Plastic Calcium Borate, Borocalcite

OxideAnalysisFormula
CaO19.35%0.878
Na2O2.97%0.122
Al2O37.17%0.179
B2O326.31%0.962
SiO221.70%0.919
LOI22.50
Oxide Weight197.29
Formula Weight254.57
If this formula is not unified correctly please contact us.

Since this material varied so much over the years, Ron Roy has been using various dated versions of the analysis, this is one of them.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Gerstley Bor (99)" descrip="Plastic Calcium Borate, Borocalcite" searchkey="" loi="0.00" casnumber="71377-02-1"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="19.350" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.970" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.170" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.310" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="22.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved