General Frit GF-8

LOW EXPANSION

Alternate Names: Frit 8, Frit GF8

Addition to glazes to reduce thermal expansion to improve resistance to crazing.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-8" descrip="LOW EXPANSION" searchkey="Frit 8, Frit GF8" loi="0.00" casnumber="65997-18-4"> </material>