General Frit GF-27

Medium lead frit cone 06-04 all-fritted hobby/artware glazes

Alternate Names: Frit 27, Frit GF27

OxideAnalysisFormula
CaO4.51%0.290
Na2O3.61%0.210
PbO30.98%0.500
Al2O33.39%0.120
B2O312.75%0.660
SiO243.71%2.620
ZrO21.02%0.030
Oxide Weight360.24
Formula Weight360.24
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.90
GSPT - Frit Softening Point 1400F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-27" descrip="Medium lead frit cone 06-04 all-fritted hobby/artware glazes" searchkey="Frit 27, Frit GF27" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.516" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.614" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.981" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.398" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.752" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.712" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="1.026" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved