General Frit GF-25

Cadmium frit for make cadmium selenium colors

Alternate Names: Frit 25, Frit GF25

OxideAnalysisFormula
CaO0.80%0.049
K2O1.50%0.055
Na2O9.50%0.530
CdO3.70%0.100
PbO17.20%0.266
Al2O33.10%0.105
B2O314.80%0.735
SiO247.00%2.703
ZrO20.60%0.017
Oxide Weight339.46
Formula Weight339.46
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.70
GSPT - Frit Softening Point 1742F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-25" descrip="Cadmium frit for make cadmium selenium colors" searchkey="Frit 25, Frit GF25" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.500" tolerance=""/> <oxide symbol="CdO" name="Cadmium Oxide" status="" percent="3.700" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="17.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved