General Frit GF-20

Clear leaded glaze for chrome-tin pink all-fritted glazes

Alternate Names: Frit 20, Frit GF20

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-20" descrip="Clear leaded glaze for chrome-tin pink all-fritted glazes" searchkey="Frit 20, Frit GF20" loi="0.00" casnumber="65997-18-4"> </material>