General Frit GF-18

Leaded calcium frit for cone 01-5 dinnerware glazes

Alternate Names: Frit 18, Frit GF18

OxideAnalysisFormula
CaO10.46%0.574
K2O2.72%0.089
Na2O1.99%0.099
PbO17.22%0.238
Al2O36.23%0.188
B2O37.83%0.347
SiO253.52%2.743
Oxide Weight307.92
Formula Weight307.92
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.30
GSPT - Frit Softening Point 1950F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-18" descrip="Leaded calcium frit for cone 01-5 dinnerware glazes" searchkey="Frit 18, Frit GF18" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.462" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.726" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.994" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="17.224" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.231" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.833" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.529" tolerance=""/> </oxides> </material>