General Frit GF-154

HIGH STRONTIUM BOROSILICATE

Alternate Names: Frit 154, Frit GF154

A 'specific-oxide' borosilicate frit (contains only strontium, boron, silica).
A cone 06 glaze additive to supply SrO.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-154" descrip="HIGH STRONTIUM BOROSILICATE" searchkey="Frit 154, Frit GF154" loi="0.00" casnumber="65997-18-4"> </material>