General Frit GF-144

Low expansion high magnesia borosilicate frit

Alternate Names: Frit 144, Frit GF144

Used in partially-fritted dinnerware and artware glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-144" descrip="Low expansion high magnesia borosilicate frit" searchkey="Frit 144, Frit GF144" loi="0.00" casnumber="65997-18-4"> </material>