General Frit GF-136

High Potassium

Alternate Names: Frit 136, Frit GF136

OxideAnalysisFormula
CaO0.71%0.040
K2O7.32%0.247
Na2O13.11%0.673
ZnO1.02%0.040
Al2O312.91%0.403
B2O316.77%0.767
SiO248.17%2.550
Oxide Weight318.15
Formula Weight318.15
If this formula is not unified correctly please contact us.

Used in partially-fritted dinnerware and artware glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-136" descrip="High Potassium" searchkey="Frit 136, Frit GF136" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.710" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.320" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.110" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.020" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.910" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.770" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.170" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved