General Frit GF-134

High Alkali Leadless Low Boron

Alternate Names: Frit 134, Frit GF134

OxideAnalysisFormula
CaO6.26%0.293
K2O2.17%0.060
Na2O15.27%0.647
Al2O33.53%0.091
B2O32.68%0.101
SiO270.08%3.061
Oxide Weight262.50
Formula Weight262.50
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.00
GSPT - Frit Softening Point 1400F

This frit has a very low melting point.
Low boron for artware glazes and brick coatings. Also used in crystalline glazes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-134" descrip="High Alkali Leadless Low Boron" searchkey="Frit 134, Frit GF134" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.260" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.170" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.270" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.530" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.680" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.080" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved