General Frit GF-129

High barium borosilicate leadless frit

Alternate Names: Frit 129, Frit GF129

OxideAnalysisFormula
BaO26.51%0.660
Na2O5.52%0.340
Al2O35.34%0.200
B2O312.40%0.680
SiO250.23%3.190
Oxide Weight381.74
Formula Weight381.74
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.80
GSPT - Frit Softening Point 1750F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-129" descrip="High barium borosilicate leadless frit" searchkey="Frit 129, Frit GF129" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="26.510" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.520" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.340" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.230" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved