General Frit GF-115

High Calcium Boron Leadless for partially-fritted tile glazes

Alternate Names: Frit 115, Frit GF115

OxideAnalysisFormula
CaO11.43%0.680
Na2O5.95%0.320
Al2O311.92%0.390
B2O323.15%1.110
SiO247.55%2.640
Oxide Weight333.65
Formula Weight333.65
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.90
GSPT - Frit Softening Point 1800F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-115" descrip="High Calcium Boron Leadless for partially-fritted tile glazes" searchkey="Frit 115, Frit GF115" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.430" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.950" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.920" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.150" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.550" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved