General Frit GF-113

Leadless High Boron/lime Glaze Frit

Alternate Names: Frit 113, Frit GF113

OxideAnalysisFormula
CaO14.09%0.690
K2O0.69%0.020
Na2O6.54%0.290
Al2O310.02%0.270
B2O314.44%0.570
SiO254.23%2.479
Oxide Weight274.78
Formula Weight274.78
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.00
GSPT - Frit Softening Point 1600F

Used for both all-fritted and partially-fritted dinnerware and artware glazes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-113" descrip="Leadless High Boron/lime Glaze Frit" searchkey="Frit 113, Frit GF113" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.090" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.690" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.540" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.020" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.440" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.230" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved