General Frit GF-111

SODIUM CALCIUM BOROSILICATE

Alternate Names: Frit 111, Frit GF111

OxideAnalysisFormula
CaO20.04%0.683
Na2O10.28%0.317
B2O323.30%0.640
SiO246.37%1.475
Oxide Weight191.18
Formula Weight191.18
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.60
GSPT - Frit Softening Point 1450F

A lime and borate source in partially fritted glazes, lead bisilicate glazes and low cost hobby glazes cone 02-10.

Low alumina makes room for blending kaolin to harden the glaze and impart excellent application properties.

See also: TAM C-14


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-111" descrip="SODIUM CALCIUM BOROSILICATE" searchkey="Frit 111, Frit GF111" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="20.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.280" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.370" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved