General Frit GF-103

Calcium sodium borosilicate for partially fritted tile glazes

Alternate Names: Frit 103, Frit GF103

OxideAnalysisFormula
CaO16.91%0.680
K2O0.41%0.010
Na2O8.52%0.310
Al2O34.97%0.110
B2O318.82%0.610
SiO250.35%1.890
Oxide Weight225.58
Formula Weight225.58
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.80
GSPT - Frit Softening Point 1800F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="General Frit GF-103" descrip="Calcium sodium borosilicate for partially fritted tile glazes" searchkey="Frit 103, Frit GF103" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="16.911" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.418" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.520" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.974" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.821" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.355" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved