G&W Kingston Clay

Semi plastic terra cotta clay

OxideAnalysisFormula
CaO0.20%0.017
MgO0.60%0.069
K2O2.60%0.128
Na2O0.50%0.037
TiO20.60%0.035
Al2O322.00%1.000
SiO255.00%4.243
Fe2O310.70%0.310
LOI7.70
Oxide Weight427.47
Formula Weight463.13
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="G&W Kingston Clay" descrip="Semi plastic terra cotta clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="10.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="7.700" tolerance=""/> </volatiles> </material>