G-200 EU Feldspar

G200 equivalent from Spain

OxideAnalysisFormula
CaO0.50%0.055
MgO0.08%0.012
K2O11.00%0.723
Na2O2.10%0.210
TiO20.03%0.002
Al2O317.00%1.032
SiO268.50%7.056
Fe2O30.10%0.004
LOI0.50
Oxide Weight614.76
Formula Weight617.85
If this formula is not unified correctly please contact us.

This is being sold by Imerys as an equivalent to G200 Feldspar (because the mine of the latter is being closed during 2013 because the deposit is depleted). The data sheet says it is obtained from a feldspathic sand by a flotation process.

It is 70% K Feldspar, 23% Na Feldspar, 7% quartz.

Particle size:
+200 mesh: 0.5%
+325 mesh: 6.2%

On paper the chemistry is pretty similar to G-200.
Laguna Clay is now selling Mahavir Feldspar from India as the G200 equivalent.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="G-200 EU Feldspar" descrip="G200 equivalent from Spain" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.080" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="11.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.030" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.500" tolerance=""/> </volatiles> </material>