Fusion Frit FZ-583

Barium Zinc Zero Boron frit

Alternate Names: Frit FZ583

OxideAnalysisFormula
BaO37.00%0.505
K2O1.50%0.033
Na2O1.50%0.051
ZnO16.00%0.411
Al2O34.00%0.082
SiO240.00%1.392
Oxide Weight209.19
Formula Weight209.19
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-583" descrip="Barium Zinc Zero Boron frit" searchkey="Frit FZ583" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="37.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="16.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved