Fusion Frit FZ-580

Fast fire zinc opaque frit

Alternate Names: Fusion Frit FZ 580

OxideAnalysisFormula
CaO10.60%0.388
MgO3.00%0.153
K2O4.80%0.105
Na2O1.60%0.053
ZnO12.00%0.302
Al2O36.20%0.125
B2O32.00%0.059
SiO249.80%1.699
ZrO210.00%0.166
Oxide Weight205.10
Formula Weight205.10
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.8 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-580" descrip="Fast fire zinc opaque frit" searchkey="Fusion Frit FZ 580" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.600" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.800" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="10.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved