Fusion Frit FZ-576

Ca-Zn transparent monoporosa frit

Alternate Names: Fusion Frit FZ576

OxideAnalysisFormula
CaO10.00%0.418
K2O2.10%0.052
Na2O5.00%0.189
ZnO11.80%0.340
Al2O35.80%0.133
B2O34.30%0.145
SiO261.00%2.382
Oxide Weight234.66
Formula Weight234.66
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.2 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-576" descrip="Ca-Zn transparent monoporosa frit" searchkey="Fusion Frit FZ576" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="11.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved