Fusion Frit FZ-565

CaZn frit for slow fire

Alternate Names: Fusion Frit FZ565

OxideAnalysisFormula
CaO13.50%0.492
MgO0.50%0.025
K2O0.50%0.011
Na2O5.80%0.191
ZnO11.20%0.281
Al2O38.50%0.170
B2O31.50%0.044
SiO258.50%1.989
Oxide Weight204.29
Formula Weight204.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.78 x 10-6
GSPT - Frit Softening Point 1550F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-565" descrip="CaZn frit for slow fire" searchkey="Fusion Frit FZ565" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.800" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="11.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="1.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved